Research Article

Development of High-Performance UV Detector Using Nanocrystalline Diamond Thin Film

Figure 3

The surface roughness and contact angle values with water for the diamond films grown under various working pressures of 40, 60, and 80 Torr, respectively.
492152.fig.003a
(a) 40 Torr
492152.fig.003b
(b) 60 Torr
492152.fig.003c
(c) 80 Torr
492152.fig.003d
(d) 40 Torr
492152.fig.003e
(e) 60 Torr
492152.fig.003f
(f) 80 Torr