Research Article
Boundary Layer of Photon Absorption Applied to Heterogeneous Photocatalytic Solar Flat Plate Reactor Design
Table 2
Average optical properties of commercial photocatalysts based on titanium dioxide under solar radiation.
| Catalyst | ×10−4 (cm2 g−1) | ×10−3 (cm2 g−1) | ×10−4 (cm2 g−1) | | |
| Aldrich | 3.73 | 2.43 | 3.98 | 0.94 | 0.84 | Degussa | 5.42 | 2.87 | 5.71 | 0.95 | 0.87 | Merck | 2.97 | 2.68 | 3.24 | 0.92 | 0.81 | Hombikat | 2.52 | 1.17 | 2.64 | 0.96 | 0.88 | Fischer | 1.60 | 2.65 | 1.86 | 0.86 | 0.72 | Fluka | 1.64 | 2.89 | 1.92 | 0.85 | 0.71 |
|
|