Research Article
Effect of the Mg/Al Ratio on Activated Sol-Gel Hydrotalcites for Photocatalytic Degradation of 2,4,6-Trichlorophenol
Table 2
Kinetics of degradation.
| Catalyst | k (min−1) | t1/2 (min) | Degradation (%) |
| HT-1 500°C | 0.0186 | 37.27 | 94.18 | HT-2 500°C | 0.0158 | 43.87 | 92.49 | HT-4 500°C | 0.0102 | 67.96 | 86.15 | HT-5 500°C | 0.0094 | 73.74 | 84.25 | HT-7 500°C | 0.0054 | 128.36 | 63.89 |
|
|