Textural data and values of TiO2, W-TiO2, and W-.

Samples (m2/g) (Å) (cm3/g) (eV)

TiO2140390.213.20
W-TiO2126380.203.06
W-TiO2/SiO2432290.213.06

: surface area obtained by BET method; : average pore size; : pore volume; : gap band energy.