Research Article
Crystalline Silicon PERC Solar Cell with Ozonized AlOx Passivation Layer on the Rear Side
Figure 8
Minority carrier lifetime versus minority carrier density for the ozone-treated bare wafer (top) and the ozone-treated commercial blue wafer (bottom) both annealed at 600°C for 90 seconds. The specified carrier density is 1015 cm-3.