Table 1: Effect of changes in Cc on primary structural parameters of PAA xerogels.

Cc, wt% , g/mol , mol/m3 , nm

0.0153.135.083239−0.499
0.0242.516.506203−0.497
0.0351.958.472170−0.503
0.0491.6610.149152−0.503
0.0601.5111.261142−0.502