Table 3:
Effect of changes in Cc on primary structural parameters of PMA xerogels.
Cc, wt%
·10
−5
, g/mol
·10
4
, mol/cm
3
, nm
0.015
2.7
3.5
290
0.024
2.2
4.2
250
0.035
1.4
6.7
180
0.049
0.91
10.4
132
0.060
0.75
11.7
118