Table 5:
The effect of Cc on primary structural parameters of PAAG xerogels.
Cc, wt%
𝑀
𝑐
·10
−6
, g/mol
𝜌
𝑐
, mol·10
3
/cm
3
𝑑
, nm
0.4
1.59
0.80
503
0.6
1.27
1.08
426
0.8
0.82
1.73
310
1.0
0.72
2.03
284
1.2
0.46
3.34
205