Research Article

Effect of Sisal Fiber Surface Treatment on Properties of Sisal Fiber Reinforced Polylactide Composites

Figure 3

Flexural properties of 30 wt.% surface-treated Sisal fibers compared to untreated Sisal fibers reinforced composites.
803428.fig.003