Table 3:
Damping characteristics of PLA-g-MDI composites.
Sample
intensity at peak
temperature at peak (°C)
Damping reduction (%)
PLA-g-MDI
0,233
77.3
—
PLA-g-MDI/Mica
0,258
80.8
−10.5
PLA-g-MDI/Zeolite
0,207
77.3
+11.1
PLA-g-MDI/Vansil
0,250
75.8
−7.2