Enzyme-Mediated Ring-Opening Polymerization of Pentadecalactone to Obtain Biodegradable Polymer for Fabrication of Scaffolds for Bone Tissue Engineering
Figure 8
MWD curves calculated from GP chromatograms: (a)—sample 22 (control), (b)—sample 23 ([M]/[HEMA] = 20 mol. ratio), (c)—sample 24 ([M]/[HEMA] = 40 mol. ratio); for details, see Table 6.