Research Article

Enzyme-Mediated Ring-Opening Polymerization of Pentadecalactone to Obtain Biodegradable Polymer for Fabrication of Scaffolds for Bone Tissue Engineering

Table 3

EMROP of pentadecalactone. Dependence of product yield and polymer intrinsic viscosity on reaction time.

Sample numberTime, hYield, %[η], dL/g

928930.21
84920.38

Conditions: CALB; 65°C; [M]/[E] = 10/1 wt./wt.; [M] concentration—50 wt.%.