Research Article

Heat Treatment Effects on the Mechanical Properties and Morphologies of Poly (Lactic Acid)/Poly (Butylene Adipate-co-terephthalate) Blends

Table 3

The enthalpy and crystallinity of PLA/PBAT blends treated at 100°C for 8 and 24 hr.

Code
0 hr8 hr24 hr
(J/g) (%) (J/g) (%) (J/g) (%)

PLA3742.4439.4743.4431.5934
PLA/PBAT (70/30)22.3832.324.0333.321.2332.61
PLA/PBAT (50/50)16.5833.7216.3235.115.6833.72
PLA/PBAT (30/70)9.9134.629.6634.629.1432.76

: The crystal melting enthalpy of PLA.
: The degree of crystallinity ( ) of PLA.