Research Article
Comparative Analysis of the Effect of Organoclay, Boron Nitride, and Fluoropolymer on the Rheology and Instabilities in the Extrusion of High Density Polyethylene
Figure 9
HDPE extrudate at a shear rate of 87 s−1 (stick-slip region) and (b) at a shear rate of 144 s−1 (gross-melt fracture region).
(a) |
(b) |