Research Article
A Study on Physical Performance for Poly(L-lactic acid) in Addition to Layered Strontium Phenylphosphonate
Table 1
DSC data of PLLA and PLLA/SrP samples at a cooling rate of 1°C/min.
| Sample | Rate/°C/min | /°C | /°C | /J·g−1 | /°C |
| PLLA | 1 | 101.4 | 94.5 | 0.1 | — |
| PLLA/0.3% SrP | 1 | 111.6 | 107.1 | 30.7 | 145.8 | PLLA/0.7% SrP | 1 | 116.3 | 109.4 | 31.0 | 146.2 | PLLA/1% SrP | 1 | 117.1 | 110.1 | 30.6 | 146.9 | PLLA/1.5% SrP | 1 | 116.9 | 110.1 | 30.4 | 146.8 |
|
|