Characterization of Alkaline Treatment and Fiber Content on the Physical, Thermal, and Mechanical Properties of Ground Coffee Waste/Oxobiodegradable HDPE Biocomposites

Figure 4

SEM image of (a) 0 hr, (b) 1 hr, (c) 6 hr, (d) 12 hr, and (e) 24 hr of 1% NaOH treated GCW.
(a)
(b)
(c)
(d)
(e)