Research Article

Facile Preparation of Biocomposite from Prawn Shell Derived Chitosan and Kaolinite-Rich Locally Available Clay

Table 4

Temperature profile and weight variation of the materials.

MaterialTemperature (°C)(Weight %)
Moisture removalVolatile and organic matter removalDegradation temperatureWeight loss at 600°C

CHT50–200200–35055
MCUp to 100Not mentionable6
SB-150–150256–360Above 30053
SB-250–150256–360Above 35050
SB-350–150256–360Above 30045
SB-450–150256–360Above 35044
SB-5Below 100240–300Two steps: 450–500
500–600
37