Research Article

Sulfate and Calcium Chloride Resistance of Steel/Glass Fiber-Reinforced Polymer Hybrid Panel for Improved Movable Weir Application

Figure 16

Fracture deformation with thickness of hybrid panels after Na2SO4 solution immersions.
(a) 9.2 mm (plain)
(b) 12.2 mm (plain)
(c) 15.2 mm (plain)
(d) 9.2 mm (sand blast)
(e) 12.2 mm (sand blast)
(f) 15.2 mm (sand blast)