Flexural Assessment of Blast-Damaged RC Beams Retrofitted with CFRP Sheet and Steel Fiber
Table 10
Static flexural test results.
| Variables | Max. load (kN) | Flexural strength (kN·m) | Ductility index (Фu/Фy) | Intact | Damaged | Repaired | Intact | Damaged | Repaired | Intact | Damaged | Repaired |
| NC-D10-S100 | 196.5 | 79.3 | 217.6 | 186.7 | 75.3 | 206.7 | 7.9 | 1.3 | 4.4 | NC-D10-S50 | 194.6 | 134.6 | 205.8 | 184.9 | 127.9 | 195.5 | 4.8 | 3.1 | 6.1 | NC-D13-S100 | 186.9 | 113.3 | 212.3 | 177.6 | 107.6 | 201.7 | 7.3 | 1.4 | 8.7 | NC-D10-S100-F | 217.5 | 105.9 | 258.4 | 206.6 | 100.6 | 245.5 | 3.3 | 1.9 | 9.1 | SFRC-D10-S100 | 207.5 | 137.2 | 225.3 | 197.1 | 130.3 | 225.3 | 11.5 | 2.7 | 5.5 |
|
|