Research Article
A Study of the Deformation, Network, and Aging of Polyethylene Oxide Films by Infrared Spectroscopy and Calorimetric Measurements
Table 1
Characteristics of the melting traces of the PEO sample in different conditions.
| |||||||||||||||||||||||||||||||||||||||||||||||||
a The value of c is found to be 0.72 from ΔH0 = 204 J/g. b The value of ΔHrelax and the range of Trelax are sensitive to the conditions [22–30, 36, 37]. c The signal in the melt is endothermic for a deformation and exothermic for a relaxation. |