Table 1: The mechanical properties of the specimen.

Dir.Thick.
(mm)
Rp0,2
(MPa)
Rm
(MPa)
A80
(%)

0,7512429744,51,70,25
45°0,75139305421,60,23
90°0,7513229043,52,30,24