Research Article

Effect of Cryosoaking Time on Transition in Wear Mechanism of M2 Tool Steel

Figure 12

Worn surface of HTC (4 hrs) depicts mild-stable transition wear with shallow grooving along the sliding direction with indication of carbides and pits due to delamination wear mode.
408016.fig.0012