Research Article

Relationship between Surface Abrasion Wear and Brightness in Glazed Porcelainized Stoneware Tiles

Figure 5

OM micrographs (top views) of bright glazed surfaces coated with the protective layer, P20C composition deposited in half-sphere geometry, after 𝑁 cycles of abrasion: (a) 150 cycles, (b) 300 cycles, (c) 800 cycles, (d) 2,000 cycles, (e) 4,000 cycles, and (f) 6,000 cycles. Magnification: 20x. Not etched.
548129.fig.005a
(a)
548129.fig.005b
(b)
548129.fig.005c
(c)
548129.fig.005d
(d)
548129.fig.005e
(e)
548129.fig.005f
(f)