Research Article

Study of Mushy-Zone Development in Dendritic Microstructures with Glass-Forming Eutectic Matrices Using Electrostatic Levitation

Figure 3

SEM micrographs of representative areas of processed samples from coarsening study, overlaid with processed and segmented version of each micrograph. Alloys and hold times as indicated. Note that the glass-forming matrix crystallized after ESL processing due to the inherently low cooling rates in the apparatus.
108363.fig.003a
(a)
108363.fig.003b
(b)
108363.fig.003c
(c)