Research Article
High Performance PEM Fuel Cell with Low Platinum Loading at the Cathode Using Magnetron Sputter Deposition
Table 2
EAS and hydrogen adsorption charge results for different configurations of sputtered Pt.
| Height of Pt sputtered (Å) | Electrochemical active surface (EAS) | Hydrogen adsorption charge | Glass carbon area | EAS (cm2/g) | Qhm (mC/cm2) | Qhm1 (mC) | S (cm2) |
| 223.2 Å (0.05 mg/cm2) | 52.3176 | 0.5493 | 0.0388 | 0.0707 | 2*111.6 Å (0.05 mg/cm2) | 82.7137 | 0.8685 | 0.0614 | 0.0707 | 2*67 Å + 89.2 Å (0.05 mg/cm2) | 142.8164 | 1.4996 | 0.1059 | 0.0707 |
|
|