Research Article

Conductivity and Complex Electrical Formalism of the Iron-Doped PbLaTiO3 Ferroelectric Relaxor

Figure 2

SEM micrographs of the PL12FxT ( in (a) and 3% in (b)) ceramics sintered in 1200°C for 2 h and their EDX spectra.
231302.fig.002a
(a)
231302.fig.002b
(b)