Infiltration Kinetics of Wetting in a Building Plaster and the Effect of Added Glass and Hemp Fibers

Table 7

Capillary moisture content ( ) and saturated moisture content ( ).

= /

Plaster0.311 ± 0.0100.335 ± 0.01092.8%
PGF0.309 ± 0.0100.332 ± 0.01093.0%
PHF0.296 ± 0.0100.325 ± 0.01091.1%