Effect of Cryosoaking Time on Transition in Wear Mechanism of M2 Tool Steel
Figure 12
Worn surface of HTC (4 hrs) depicts mild-stable transition wear with shallow grooving along the sliding direction with indication of carbides and pits due to delamination wear mode.