Seismic Behaviour of Exterior Reinforced Concrete Beam-Column Joints in High Performance Concrete Using Metakaolin and Partial Replacement with Quarry Dust
Table 1
Details of test specimens.
Sl. number
Specimens ID
Description of test specimens
% of metakaolin and quarry dust
1
O1 & O2
Conventional concrete (without seismic detailing)
ā
2
SS1 & SS2
Conventional concrete (with seismic detailing)
ā
3
E11 & E12
High performance concrete (without seismic detailing)
Normal concrete + 10% metakaolin + 30% quarry dust
4
E21 & E22
High performance concrete (with seismic detailing)
Normal concrete + 10% metakaolin + 30% quarry dust
5
E31 & E32
High performance concrete (with seismic detailing) (confinement joint)
Normal concrete + 10% metakaolin + 30% quarry dust