Table 1:
The index and thickness of both the top layer and the TMS film of oxygen-treated plasma-polymerized film at 632.8 nm.
Day
Top layer
TMS film
Index
Thickness (nm)
Index
Thickness (nm)
1
1.51959
7.1
1.6815
95.4
7
1.55123
8.1
1.659
95.7
15
1.553
8.8
1.6465
96.3
50
1.5799
13.7
1.624
93.9