Research Article

Mineral-Oxide-Doped Aluminum Titanate Ceramics with Improved Thermomechanical Properties

Table 3

Comparison of CTE values and hysteresis area.

Sample Id%TD%AT phaseCTE value (30–1000°C )Hysteresis area (cm2)

C085.1392.04 /°C91
C398.998 /°C68
C598.6395.5 /°C95