Increasing Bending Strength of Porcelain Stoneware via Pseudoboehmite Additions
Figure 3
X-ray diffraction patterns of experimental porcelain compositions fired at 1200°C for boehmite additions (2, 5, 10 wt%). *Note moderate increase in the mullite peaks intensity.