Textural properties of samples Ta, Tb, and LTO.
| Sample | /m2 g−1 | /cm3 g−1 | Average pore size/nm |
| Ta | 413.35 | 0.1920 | 2.21 | Tb | 182.74 | 0.2754 | 4.36 | LTO600 | 22.37 | — | — | LTO700 | 17.19 | 0.0370 | 1.52 | LTO800 | 10.61 | — | — |
|
|