Research Article
Fabrication of Antimicrobial Perspiration Pads and Cotton Cloth Using Amaranthus dubius Mediated Silver Nanoparticles
Table 1
Comparative results of methods used in the fabrication of AgNPs on the cotton cloth and perspiration pad samples.
| S. No. | Method | Time (minutes) | Weight of the cotton cloth (g) | Weight of the perspiration pad (g) | Before | After | Difference in weight | Before | After | Difference in weight |
| 1. | Dipping | 60 | 0.05250 | 0.05364 | 0.00114 | 0.0451 | 0.04838 | 0.00328 |
| 2. | Sonication | 30 | 0.05070 | 0.05275 | 0.00205 | 0.0479 | 0.05190 | 0.00409 | 60 | 0.05160 | 0.05390 | 0.00230 | 0.0425 | 0.04704 | 0.00454 | 90 | 0.05170 | 0.05664 | 0.00494 | 0.0425 | 0.04957 | 0.00707 |
| 3. | Control | 30 | 0.05315 | 0.05485 | 0.00170 | 0.0330 | 0.03551 | 0.00242 |
|
|
Bold values refer to the highest amount of coating onto the cotton cloth and perspiration pads.
|