Research Article

Hot-Dip Aluminizing of Low Carbon Steel Using Al-7Si-2Cu Alloy Baths

Figure 2

Intermetallic layer formed between substrate and Al-Si topcoat for dipping times of (a) 300 s and (b) 2400 s at 690°C temperature.
180740.fig.002a
(a)
180740.fig.002b
(b)