Research Article

Effect of Testing Rate on Adhesion Properties of Acrylonitrile-Butadiene Rubber/Standard Malaysian Rubber Blend-Based Pressure-Sensitive Adhesive

Figure 5

Variation of peel strength (180° peel test) with testing rate for NBR/SMR L blend-based adhesive at various coating thicknesses.
519416.fig.005