Research Article

Effect of Testing Rate on Adhesion Properties of Acrylonitrile-Butadiene Rubber/Standard Malaysian Rubber Blend-Based Pressure-Sensitive Adhesive

Figure 7

Variation of peel strength (90° peel test) with coating thickness for various testing rates.