Research Article
Plasticized Biodegradable Poly(lactic acid) Based Composites Containing Cellulose in Micro- and Nanosize
Table 2
Thermal properties measured by DSC.
| | melt peaks (°C) | (°C ) | (°C ) | (J/g) | (J/g) | (%) |
| | 143.5 | 151.6 | 43.9 | 102.8 | 33.76 | 21.41 | 13.19 | | 134.2 | 150.1 | 41.2 | 97.3 | 31.46 | 7.95 | 25.12 | | 138.6 | 150.7 | 40.9 | 92.8 | 28.29 | 11.13 | 18.33 | | 135.4 | 149.9 | 41.5 | 83.4 | 27.48 | 6.64 | 22.26 | | 137.2 | 150.1 | 42.0 | 88.6 | 28.74 | 11.30 | 18.63 | | 137.8 | 150.3 | 41.1 | 89.7 | 28.89 | 9.17 | 21.07 | | — | 150.5 | 42.3 | 90.3 | 29.24 | 7.52 | 23.21 | | 138.6 | 150.5 | 42.5 | 91.6 | 30.11 | 5.59 | 26.20 |
|
|