Research Article

Surface Characteristics and High Cycle Fatigue Performance of Shot Peened Magnesium Alloy ZK60

Figure 3

TEM images and corresponding SAED patterns of ZK60 alloy after SP at Almen intensity of 0.10 mmN: (a) bright field image and (b) its magnification about 10 μm depth; (c) bright field image and SAED pattern as well as (d) its dark field image about 20 μm depth.
682191.fig.003a
(a)
682191.fig.003b
(b)
682191.fig.003c
(c)
682191.fig.003d
(d)