Amorphization, Crystallization, and Magnetic Properties of Melt-Spun Alloys

Figure 6

MFM image of SmCo6.8(Cr3C2)0.2 ribbon annealed at 650°C for 5 min in the thermally demagnetized state (a) and the corresponding AFM image (b).