Research Article
Developing 1D MM of Axisymmetric Transient Quenched Chromium Steel to Determine LHP
Table 3
Cooling time, cooling rate, Jominy distance, and HRC for the nodes to , water cooled.
| Node | (s) | ROC (°Cs) | Jominy distance (mm) | Hardness (HRC) |
| | 8.245 | 36.38568 | 8.685 | 59.297 | | 8.138 | 36.864094 | 8.621 | 59.359 | | 7.406 | 40.507696 | 8.179 | 59.775 | | 5.311 | 56.486537 | 6.935 | 60.316 | | 1.93 | 155.44041 | 3.431 | 61.421 |
|
|