Retention times recorded for N2 and Kr separated on example carbon molecular sieves originated from Salix viminalis wood.

(°C)
Gas7060504030
± ± ± ± ±

Carbon SV6163

Kr154441.7177023.2212877.3265447.43393176.2
N24871.55261.05671.86418.07371.0

Carbon DSV6161

Kr8867.810394.5128564.5150729.9175815.3
N23862.74122.74591.65040.85514.6