Research Article

Giant Improvement on the Afterglow of Sr4Al14O25:Eu2+,Dy3+ Phosphor by Systematic Investigation on Various Parameters

Figure 7

EDS mapping of Eu ((a), (c), and (e)) and Dy ((b), (d), and (f)) in strontium aluminate phosphors prepared with different H3BO3 concentrations: ((a), (b)) 0 mol%, ((c), (d)) 40 mol%, and ((e), (f)) 100 mol%.
613090.fig.007a
(a)
613090.fig.007b
(b)
613090.fig.007c
(c)
613090.fig.007d
(d)
613090.fig.007e
(e)
613090.fig.007f
(f)