Research Article

Investigations of Different Phases Responsible for Changes in Optical Properties of Organic Semiconducting Device Material Thin Films

Figure 7

Infrared transmission spectra (in arbitrary unit) of environmentally exposed Znq2 thin films deposited at different rates of 1, 1.5, 2.0, and 2.5 Å/s.
690237.fig.007