Research Article

Investigations of Different Phases Responsible for Changes in Optical Properties of Organic Semiconducting Device Material Thin Films

Figure 8

Photoluminescence peak shift from 540 nm in pristine thin film to 500 nm in environmentally exposed film deposited at 1 Å/s.
690237.fig.008