A typical run of malachite green dye degradation using cerium-cadmium oxidea.

Time (min.)Optical Density (O.D.)

0.001.2402.0934
20.000.5601.7482
40.000.2131.3284
60.000.0770.8865
80.000.0360.5563

Reaction conditions: dye concentration =  M, light intensity = 600  , cerium-cadmium oxide = 0.03 g in 50 mL dye solution, and pH = 8.