Research Article

Synthesis of Thin Films by Magnetron Sputtering

Figure 4

AFM images taken before ((a) and (b)) and after indentation ((c) and (d)). Although ReN3 is a brittle material, there are no traces of the indentation remaining in the surface.
745736.fig.004a
(a)
745736.fig.004b
(b)
745736.fig.004c
(c)
745736.fig.004d
(d)