Research Article

Synthesis and Study of CdS Thin Films Prepared with Different KMnO4 Activation Time

Figure 4

SEM micrograph of CdS thin film by CBD for different glass substrate activation time 5 min, 10 min, 15 min, 20 min, 25 min, and 30 min.