Research Article

Modification of Aluminium 6063 Microstructure by Adding Boron and Titanium to Improve the Thermal Conductivity

Table 3

Titanium addition to Aluminium 6063.

Specimen reference Ti wt%

Ti-10.1
Ti-20.3
Ti-30.5
Ti-41
Ti-51.5
Ti-62
Ti-72.5
Ti-83