Bulk Behavior of Ball Milled AA2124 Nanostructured Powders Reinforced with TiC

Table 2

Effect of TiC additions to the micron and nanopowder matrices.

TiC wt%Compressive strength (MPa) (micronpowder matrices)Compressive strength (MPa) (nanopowder matrices)

0313.66389
5357.84493.23
10415.55538.57
20373.65507.47